ABSTRACT:
Coatings are described which are particularly suited for the protection of nickel and cobalt superalloy articles at elevated temperatures. The protective nature of the coatings is due to the formation of an alumina layer on the surface of the coating which serves to reduce oxidation/corrosion. The coatings contain aluminum, chromium, yttrium (or other oxygen active elements) and a metal chosen from the group consisting of nickel, cobalt and iron or mixtures thereof. The coatings further contain a controlled percentage of silicon which serves to greatly improve the protection afforded by the alumina film to the surface of the coating.
REFERENCES:
patent: 3741791 (1973-06-01), Maxwell et al.
patent: 3869779 (1975-03-01), Gedwill et al.
Rutledge L. Dewayne
Sohl Charles E.
United Technologies Corporation
Weise E. L.
LandOfFree
Superalloy base having a coating containing silicon for corrosio does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Superalloy base having a coating containing silicon for corrosio, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Superalloy base having a coating containing silicon for corrosio will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-578732