ABSTRACT:
The leaching efficiency of nickeliferous lateritic ore is optimized by scalping the ore to remove a coarse low-nickel fraction and provide a fine nickel-rich fraction which is then high pressure leached in a sulfuric acid solution by controlling the parameters temperature, pulp density, the rate of acid addition, leaching time, agitation rate, etc., whereby a pregnant solution is obtained with the nickel to (Fe+Al+Cr) ratio exceeding about 2.
REFERENCES:
patent: 2842436 (1958-07-01), Dasher et al.
patent: 3761566 (1973-09-01), Michal
Queneau, Editor, Extractive Metallurgy of Copper, Nickel, Cobalt Interscience, New York, (1961), pp. 363-397.
Boldt et al., The Winning of Nickel, Longmans Canada Ltd., (1967), pp. 290-294, 388, 437-444.
Chou Eddie C.
Queneau Paul B.
Amax Inc.
Hearn Brian E.
Kalil Eugene J.
Serijan Kasper T.
Vertiz O. R.
LandOfFree
Sulfuric acid leaching of nickeliferous laterite does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Sulfuric acid leaching of nickeliferous laterite, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Sulfuric acid leaching of nickeliferous laterite will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2315746