Stock material or miscellaneous articles – All metal or with adjacent metals – Composite; i.e. – plural – adjacent – spatially distinct metal...
Reexamination Certificate
2007-11-13
2007-11-13
LaVilla, Michael E. (Department: 1775)
Stock material or miscellaneous articles
All metal or with adjacent metals
Composite; i.e., plural, adjacent, spatially distinct metal...
C428S652000, C428S633000, C416S24100B, C427S250000, C427S295000, C427S453000, C427S455000
Reexamination Certificate
active
11073529
ABSTRACT:
A protected article includes a substrate having a surface, and a protective system overlying and contacting a first portion of the surface of the substrate. The protective system has a nickel-base superalloy bond coat, an aluminide layer overlying and contacting the bond coat, and a dense vertically microcracked ceramic thermal barrier coating overlying and contacting the aluminide layer.
REFERENCES:
patent: 5035958 (1991-07-01), Jackson et al.
patent: 5236745 (1993-08-01), Gupta et al.
patent: 5403669 (1995-04-01), Gupta et al.
patent: 5520516 (1996-05-01), Taylor et al.
patent: 5562998 (1996-10-01), Strangman
patent: 5743013 (1998-04-01), Taylor et al.
patent: 5879753 (1999-03-01), Zajchowski et al.
patent: 6180262 (2001-01-01), Freling et al.
patent: 6233822 (2001-05-01), Grossklaus, Jr. et al.
patent: 6555179 (2003-04-01), Reeves et al.
patent: 6607611 (2003-08-01), Darolia
patent: 6655146 (2003-12-01), Kutter et al.
patent: 2004/0115462 (2004-06-01), Grady et al.
patent: 0496935 (1992-08-01), None
patent: 1411148 (2004-04-01), None
European Search Report mailed Jun. 20, 2007.
Nagaraj Bangalore Aswatha
Parry David Walter
Patrick D. Keith
Tomlinson Thomas John
General Electric Company
LaVilla Michael E.
LandOfFree
Substrate protected by superalloy bond coat system and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Substrate protected by superalloy bond coat system and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Substrate protected by superalloy bond coat system and... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3832260