Structure and method of manufacture for minimizing filament coup

Superconductor technology: apparatus – material – process – High temperature devices – systems – apparatus – com- ponents,... – Superconducting wire – tape – cable – or fiber – per se

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

505232, 505236, 505431, 505510, 505704, 1741251, 428212, 428379, 428697, 428698, 428702, 428930, 29599, H01B 1210, H01L 3924

Patent

active

06038462&

ABSTRACT:
A multifilamentary superconducting composite article comprising multiple substantially electrically decoupled domains, each including one or more fine, preferably twisted filaments of a desired superconducting oxide material. In a preferred embodiment, the article comprises a matrix, which substantially comprises a noble metal, a conductive jacketing layer surrounding the matrix, a plurality of discrete filament decoupling layers, each comprising an insulating material, disposed within the matrix to separate the matrix into a plurality of substantially electrically decoupled domains; a plurality of filaments, each comprising a desired superconducting oxide, which are disposed within and essentially encapsulated by the matrix and chemically isolated thereby from the decoupling layers, each of the electrically decoupled domains containing at least one filament. It provides multifilamentary articles that exhibit high DC performance characteristics and AC performance markedly superior to any currently available for these materials. The article may be manufactured by first, forming a composite intermediate comprising multiple domains, each including one or more fine, preferably twisted filaments of a superconducting oxide or its precursors and then thermomechanically processing the intermediate at conditions sufficient to produce at least one of the effects of texturing, crack healing and, if a precursor to the desired superconducting oxide remains, phase transformation in the filament material under conditions which support the electrical separation of the domains. Preferably, the forming step includes the step of providing filament decoupling layers comprising insulating materials or their predecessors to provide the desired domain separation and most preferably, the insulating material is formed in situ from its predecessor during the thermomechanical processing step. Oxide-forming predecessors are preferred, especially oxide forming materials selected from the group consisting of the transition metals, the alkaline earths, titanium, zirconium, niobium, molybdenum, aluminum, and their alloys. In a preferred embodiment, the desired superconducting oxide material is a member of the bismuth or yttrium families of oxide superconductors.

REFERENCES:
patent: 4988669 (1991-01-01), Dersch
patent: 4990491 (1991-02-01), Wagner et al.
patent: 5079218 (1992-01-01), Tanaka et al.
patent: 5102865 (1992-04-01), Woolf et al.
patent: 5122507 (1992-06-01), Yamamoto et al.
patent: 5132278 (1992-07-01), Stevens et al.
patent: 5419974 (1995-05-01), Walters et al.
patent: 5501746 (1996-03-01), Egawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Structure and method of manufacture for minimizing filament coup does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Structure and method of manufacture for minimizing filament coup, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Structure and method of manufacture for minimizing filament coup will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-178291

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.