ABSTRACT:
A formed disc for use in a low pressure rotor has a rim made of a high alloy metal of between approximately 9% and 17% chromium. The rim can be annular in shape and slide onto the perimeter of an unformed disc for the two components to be fused together, thus fabricating a formed disc. Additionally, the rim can be split into a number of components and fused together on the perimeter of a rotor disc to form a complete rim. Further, an entire disc can be made out of the high alloy metal.
REFERENCES:
patent: 2440069 (1948-04-01), Bloomberg
patent: 2918253 (1959-12-01), Mackey
patent: 3165342 (1965-01-01), Anderson
patent: 3590454 (1971-07-01), Braun
patent: 4152816 (1979-05-01), Ewing et al.
patent: 4224360 (1980-09-01), Ohnishi et al.
patent: 4633554 (1987-01-01), Clark et al.
patent: 4697987 (1987-10-01), Katayama et al.
patent: 4893388 (1990-01-01), Amos et al.
patent: 4897519 (1990-01-01), Clark et al.
patent: 5024582 (1991-06-01), Bellows et al.
patent: 5609471 (1997-03-01), Frasier et al.
Clark, R.E. et al., "Experiences with Weld Repair of Low Pressure Steam Turbine Rotors", 47th Annual Meeting of the American Power Conference, Apr. 22-24, 1985, Chicago, Illinois.
Clark, R.E. et al., "Development of the Techniques for High Pressure Rotor Weld Repair", Westinghouse Electric Corp. and Mitsubishi Heavy Industries, Ltd. Technical Seminar, Takasago, Japan, Jul. 20-22, 1987.
Milliken, C.K. et al., "Qualification Welding of 12% Chromium Segemental Vanes", Westinghouse Electric Corporation Steam Turbine -Generator Division, The Quadranagle, Orlando, FL, Technical Report TR-85039, Apr. 1, 1985.
Morin, M. and Stoeckli, "Complex Submerged Arc Weld Repairs of Large Rotating Equipment", 1994 EPRI International Conference, Mar. 23-25, 1994, Williamsburg, Virginia.
Phillips, A., ed., "Introductory Welding Metallurgy", American Welding Society, New York, 1968, pp. 118-122.
Schubert, D. et al., "Weld Repair of Geothermal Turbine Rotors a Partnering Approach", Geothermal Resources Council Transactions 1992, 16, 567-574.
Sermatech Review 1989, No. 31, pp. 1-2, "New Services for Industrial Turbines".
Metals Handbook, vol. 6, "Welding, Brazing and Soldering", 9th Edition ASM (1983).
US Patent Application, "High Chromium Content Welding Material to Improve Resistance of Corrosion Method and Device", serial No. 08/668,791, filed Jun. 24, 1996, attorney docket No. WE #58,608.
Coulon, P.A. "A Positive Experience with Large Stam Turbine Rotors Weld Repair", ASME-ASM Conference, Salt Lake City, 1985.
Amos Dennis Ray
Bachman Sallie Ann
Chen Jianqiang
Kwon John T.
Westinghouse Electric Corporation
LandOfFree
Stress corrosion resistant rims and discs for steam turbine roto does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Stress corrosion resistant rims and discs for steam turbine roto, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Stress corrosion resistant rims and discs for steam turbine roto will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-47903