Strengthened protective coatings for superalloys

Stock material or miscellaneous articles – All metal or with adjacent metals – Composite; i.e. – plural – adjacent – spatially distinct metal...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

428632, 428633, 428678, 428680, 420443, 420448, 148410, B32B 1500, C22C 1905

Patent

active

053168666

ABSTRACT:
A superalloy component includes a substrate article of a superalloy, and a strengthenable, adherent coating on the substrate. The coating is preferably a nickel-base superalloy that is strengthened by the formation of gamma and gamma-prime phases. The coating is stronger than conventional MCrAlX coatings, and, therefore, more resistant to thermal fatigue. One operable coating has a composition, in weight percent, of about 7.5 percent cobalt, about 9 percent chromium, about 6 percent aluminum, about 1 percent titanium, about 1.5 percent molybdenum, about 4 percent tantalum, about 3 percent tungsten, about 3 percent rhenium, about 0.5 percent hafnium, about 0.3 percent yttrium, about 0.5 percent columbium, about 0.05 percent carbon, about 0.015 percent boron, about 0.015 percent zirconium, and balance nickel.

REFERENCES:
patent: 4152488 (1979-05-01), Schilke et al.
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4198442 (1980-04-01), Gupta et al.
patent: 4237193 (1980-12-01), Jackson et al.
patent: 4339509 (1982-07-01), Dardi et al.
patent: 4446199 (1984-05-01), Gedwill et al.
patent: 4485151 (1984-11-01), Stecura
patent: 4758480 (1988-07-01), Hecht et al.
patent: 4769087 (1988-09-01), Genereux et al.
patent: 4921405 (1990-05-01), Wilson
patent: 4961818 (1990-10-01), Benn
patent: 4995922 (1991-02-01), Jongenburger
patent: 5035958 (1991-07-01), Jackson et al.
patent: 5043138 (1991-08-01), Darolia et al.
patent: 5068084 (1991-11-01), Cetel et al.
patent: 5077141 (1991-12-01), Naik et al.
"Metals Handbook", 9th edition, vol. 3, p. 214, TA 472 A3 1980.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Strengthened protective coatings for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Strengthened protective coatings for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Strengthened protective coatings for superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1627056

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.