ABSTRACT:
A steel resistant to intergranular stress corrosion cracking having the composition: C up to 0.20%, Si 0.05 - 0.80%, Mn 0.30 - 1.50%, P up to 0.03%, S up to 0.03%, Al (sol. Al) 0.05 - 0.25%, Zr 0.03 - 0.20%, the balance being iron and unavoidable impurities. Another intergranular stress corrosion cracking resisting steel is disclosed which contains one or both of 0.10 - 0.30% Cr and 0.10 - 0.50% Ni in addition to the composition of the first-mentioned steel.
REFERENCES:
patent: 3216823 (1965-11-01), Gulya
patent: 3259488 (1966-07-01), Nakamura
patent: 3328211 (1967-06-01), Nakamura
patent: 3666570 (1972-05-01), Korchynsky
patent: 3671336 (1972-06-01), Korchynsky
patent: 3897245 (1975-07-01), Savas
Nakazawa Toshio
Tanimura Masayuki
Tenmyo Gennosuke
LandOfFree
Steel resistant to intergranular stress corrosion cracking does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Steel resistant to intergranular stress corrosion cracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Steel resistant to intergranular stress corrosion cracking will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1445354