ABSTRACT:
High-strength, high-workability steel for cold plastic working, obtained by subjecting a hardenable carbon steel to rapid high-frequency induction heating, quenching it, rapidly heating it by high-frequency induction to a temperature of 300.degree.-600.degree. C., and rapidly cooling it. This steel can be cold plastic worked, and then reheated at 300.degree.-500.degree. C. for 30-60 minutes, to obtain a steel having a high elastic limit.
REFERENCES:
patent: 3271206 (1966-09-01), Goda et al.
patent: 3589950 (1971-06-01), Justusson
patent: 3647571 (1972-03-01), Okamoto et al.
patent: 3795550 (1974-03-01), Ettenreich et al.
patent: 3847678 (1974-11-01), Furr
patent: 3904446 (1975-09-01), Uchida et al.
patent: 3929524 (1975-12-01), Filatov et al.
patent: 3936324 (1976-02-01), Uchida et al.
patent: 4050959 (1977-09-01), Nakaoka
Hijikata Toshio
Kawasaki Kazuhiro
Neturen Company Ltd.
Skiff Peter K.
LandOfFree
Steel for cold plastic working does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Steel for cold plastic working, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Steel for cold plastic working will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-972091