ABSTRACT:
A composition of matter for inhibition of stress corrosion stainless steels in contact with aqueous and/or polar organic solutions which contain chloride ions and optionally cuprous ions, comprising an aqueous or polar organic solution of a member selected from the group consisting of quaternary ammonium alkylcarbonates and quaternary ammonium benzylcarbonates having the general formula: ##STR1##

REFERENCES:
patent: 2635100 (1953-04-01), Werntz
patent: 2648678 (1953-08-01), Heiberger
patent: 3031455 (1962-04-01), Holysz

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Stainless steels stress corrosion inhibitors does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Stainless steels stress corrosion inhibitors, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Stainless steels stress corrosion inhibitors will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-170296

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.