ABSTRACT:
A protected article includes a substrate having a substrate surface and made of a substrate nickel-base superalloy that is susceptible to the formation of a secondary reaction zone, as when contacted by an aluminum-containing layer having more than about 20 percent by weight aluminum. A protective layer contacts the substrate surface. The protective layer is of a different composition than the substrate and is made of a protective-layer nickel-base superalloy having from about 7 to about 12 percent by weight aluminum. Preferably, a thermal barrier coating system including a ceramic layer overlies and contacts the protective layer.

REFERENCES:
patent: 5151249 (1992-09-01), Austin et al.
patent: 5270123 (1993-12-01), Walston et al.
patent: 5334263 (1994-08-01), Schaeffer
patent: 5455120 (1995-10-01), Walston et al.
patent: 5482789 (1996-01-01), O'Hara et al.
patent: 5598968 (1997-02-01), Schaeffer et al.
patent: 5695821 (1997-12-01), Murphy et al.
patent: 5891267 (1999-04-01), Schaeffer et al.
patent: 5935353 (1999-08-01), Murphy et al.
patent: 6080246 (2000-06-01), Wing
patent: 6190471 (2001-02-01), Darolia et al.
patent: 6444053 (2002-09-01), Spitsberg et al.
patent: 6447932 (2002-09-01), O'Hara et al.
patent: 6468367 (2002-10-01), Mukira et al.
patent: 6471790 (2002-10-01), Fernihough
patent: 6641929 (2003-11-01), Kelly et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

SRZ-susceptible superalloy article having a protective layer... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with SRZ-susceptible superalloy article having a protective layer..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and SRZ-susceptible superalloy article having a protective layer... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3486861

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.