Spinning process for the preparation of high thermobondability p

Plastic and nonmetallic article shaping or treating: processes – Direct application of fluid pressure differential to... – Production of continuous or running length

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264143, 264168, 2642107, 2642108, 26421112, 26421114, 26421115, D01D 5092, D01D 526, D01F 606

Patent

active

056607890

ABSTRACT:
Polyolefin fibers, suitable for the preparation of nonwoven fabrics, prepared by using a spinneret or extruder with dies having a real or equivalent output diameter of the capillaries or holes greater than 0.4 mm, with the proviso that for fibers having a denier greater than or equal to 4 dtex, the ratio of the output capillary or hole diameter to the denier is greater than or equal to 0.06 mm/dtex.

REFERENCES:
patent: 4211819 (1980-07-01), Kunimune et al.
patent: 5281378 (1994-01-01), Kozulla
patent: 5318735 (1994-06-01), Kozulla

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Spinning process for the preparation of high thermobondability p does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Spinning process for the preparation of high thermobondability p, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Spinning process for the preparation of high thermobondability p will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1986174

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.