Spherical alumina particles and production process thereof

Compositions: ceramic – Ceramic compositions – Refractory

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C423S625000, C501S153000

Reexamination Certificate

active

07053018

ABSTRACT:
A process for producing roundish alumina particles includes the steps of granulating a composition containing at least one pulverized product of electrofused alumina and sintered alumina having a mean particle size of 5 to 35 μm and at least one species selected from the group consisting of a halogen compound, a boron compound and an alumina hydrate to obtain a granulated product, heating the granulated product at 1,000 to 1,600° C., and crushing the heated product.

REFERENCES:
patent: 4193768 (1980-03-01), Hasegawa et al.
patent: 4315839 (1982-02-01), Bouge et al.
patent: 4382879 (1983-05-01), Funabashi et al.
patent: 5340781 (1994-08-01), Oda et al.
patent: 0 499 585 (1992-08-01), None
patent: 0 499 585 (1992-08-01), None
patent: 0 680 929 (1995-11-01), None
patent: 0 933 397 (1999-08-01), None
patent: 05-294613 (1993-11-01), None
International Search Report for PCT/JP02/05156 dated Aug. 21, 2002.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Spherical alumina particles and production process thereof does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Spherical alumina particles and production process thereof, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Spherical alumina particles and production process thereof will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3536851

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.