Solid oxide fuel cell

Chemistry: electrical current producing apparatus – product – and – With pressure equalizing means for liquid immersion operation

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C429S010000, C429S006000, C427S115000, C252S062200, C029S623500

Reexamination Certificate

active

07745031

ABSTRACT:
SOFC cell comprising a metallic support1ending in a substantially pure electron conducting oxide, an active anode layer2consisting of doped ceria, ScYSZ, Ni—Fe alloy, an electrolyte layer3consisting of co-doped zirconia based on oxygen ionic conductor, an active cathode layer5and a layer of a mixture of LSM and a ferrite as a transition layer6to a cathode current collector7of single phase LSM. The use of a metallic support instead of a Ni—YSZ anode support increases the mechanical strength of the support and secures redox stability of the support. The porous ferrite stainless steel ends in a pure electron conducting oxide so as to prevent reactivity between the metals in the active anode which tends to dissolve into the ferrite stainless steel causing a detrimental phase shift from ferrite to austenite structure.

REFERENCES:
patent: 4209147 (1980-06-01), Jones, Jr.
patent: 4702971 (1987-10-01), Isenberg
patent: 4957673 (1990-09-01), Schroeder et al.
patent: 5021304 (1991-06-01), Ruka et al.
patent: 5064734 (1991-11-01), Nazmy et al.
patent: 5358735 (1994-10-01), Kawasaki et al.
patent: 5670270 (1997-09-01), Wallin et al.
patent: 5788788 (1998-08-01), Minh
patent: 5803934 (1998-09-01), Carter
patent: 5846664 (1998-12-01), Third et al.
patent: 5908713 (1999-06-01), Ruka et al.
patent: 6017647 (2000-01-01), Wallin et al.
patent: 6048636 (2000-04-01), Naoumidis et al.
patent: 6099985 (2000-08-01), Elangovan et al.
patent: 6232009 (2001-05-01), Batawi et al.
patent: 6248468 (2001-06-01), Ruka et al.
patent: 6280868 (2001-08-01), Badwal et al.
patent: 6458170 (2002-10-01), Visco et al.
patent: 6592787 (2003-07-01), Pickrell et al.
patent: 6605316 (2003-08-01), Visco et al.
patent: 6682842 (2004-01-01), Visco et al.
patent: 6783880 (2004-08-01), Christiansen
patent: 6843960 (2005-01-01), Krumpelt et al.
patent: 6844099 (2005-01-01), Gorte et al.
patent: 6936217 (2005-08-01), Quadadakkers et al.
patent: 6958196 (2005-10-01), Gorte et al.
patent: 7351488 (2008-04-01), Visco et al.
patent: 2001/0029231 (2001-10-01), Gorte et al.
patent: 2002/0048699 (2002-04-01), Steele et al.
patent: 2002/0122967 (2002-09-01), Gorina et al.
patent: 2002/0127455 (2002-09-01), Pham et al.
patent: 2002/0182468 (2002-12-01), Janousek et al.
patent: 2003/0015431 (2003-01-01), Barker et al.
patent: 2003/0035989 (2003-02-01), Gorte et al.
patent: 2003/0059335 (2003-03-01), Quadadakkers et al.
patent: 2003/0059668 (2003-03-01), Visco et al.
patent: 2003/0082434 (2003-05-01), Wang et al.
patent: 2003/0134171 (2003-07-01), Sarkar et al.
patent: 2003/0165726 (2003-09-01), Robert et al.
patent: 2003/0178307 (2003-09-01), Sarkar
patent: 2003/0186101 (2003-10-01), Christansen et al.
patent: 2003/0224234 (2003-12-01), Steele et al.
patent: 2003/0231973 (2003-12-01), Krumpelt et al.
patent: 2003/0232230 (2003-12-01), Carter et al.
patent: 2003/0235752 (2003-12-01), England et al.
patent: 2004/0033405 (2004-02-01), Barnett et al.
patent: 2004/0043269 (2004-03-01), Taniguchi et al.
patent: 2004/0053101 (2004-03-01), Chartier et al.
patent: 2004/0060967 (2004-04-01), Yang et al.
patent: 2004/0115503 (2004-06-01), Jacobson et al.
patent: 2004/0183055 (2004-09-01), Chartier et al.
patent: 2004/0209147 (2004-10-01), Finkenwirth et al.
patent: 2005/0089739 (2005-04-01), Seccombe et al.
patent: 2005/0181253 (2005-08-01), Finnerty et al.
patent: 2006/0024547 (2006-02-01), Waldbillig et al.
patent: 2008/0096079 (2008-04-01), Linderoth et al.
patent: 2008/0118635 (2008-05-01), Larsen
patent: 2008/0124602 (2008-05-01), Larsen et al.
patent: 2008/0142148 (2008-06-01), Nielsen et al.
patent: 2008/0166618 (2008-07-01), Larsen et al.
patent: 2440288 (2004-03-01), None
patent: 1409427 (2003-04-01), None
patent: 1997229 (2007-07-01), None
patent: 4237602 (1994-05-01), None
patent: 19650704 (1998-06-01), None
patent: 19710345 (1999-01-01), None
patent: 19836132 (2000-02-01), None
patent: 0446680 (1991-09-01), None
patent: 1065020 (2001-01-01), None
patent: 1255318 (2002-11-01), None
patent: 1306920 (2003-05-01), None
patent: 1318560 (2003-06-01), None
patent: 1383195 (2004-01-01), None
patent: 1313795 (1973-04-01), None
patent: 2400723 (2004-10-01), None
patent: 2004319286 (2004-11-01), None
patent: WO 92/15122 (1992-09-01), None
patent: WO 98/49738 (1998-11-01), None
patent: WO 99/56899 (1999-11-01), None
patent: WO 02/09116 (2002-01-01), None
patent: WO 02/073729 (2002-09-01), None
patent: WO 03/036739 (2003-05-01), None
patent: WO 03/069705 (2003-08-01), None
patent: WO 03/075382 (2003-09-01), None
patent: WO 03/105252 (2003-12-01), None
patent: WO 04/001885 (2003-12-01), None
patent: WO 2004/013925 (2004-02-01), None
patent: 2004030133 (2004-04-01), None
patent: WO 2004/030130 (2004-04-01), None
patent: 2004079033 (2004-09-01), None
patent: WO 2006/069753 (2006-07-01), None
patent: WO 2006/074932 (2006-07-01), None
patent: WO 2006/079558 (2006-08-01), None
patent: WO 2006/082057 (2006-08-01), None
patent: WO 2007/025762 (2007-03-01), None
Kim, J-H. et al., “Fabrication and characteristics of anode-supported flat-tube solid oxide fuel cell,” J. Power Sources (2003) 122(2):138-143.
Xia, C. et al., “Functionally graded cathodes for honeycomb solid oxide fuel cells,” Electrochem. Solid-State Letters (2002) 5(10):A217-A220.
Young, R.C. et al., “Symposium BB: Materials and Technologies for a Hydrogen Economy,” Materials Research Society Symposium Proceedings Series (Nov. 30, 2003) pp. 709-717.
Donald, I.W. “Preparation, properties and chemistry of glass and glass-ceramic-to-metal seals and coatings,” J. Mat. Sci. (1993) 28:2841-2886.
Dyck, C.R. et al., “Synthesis and characterization of Gd(1-x)SrxCoO(1-y)FeyO(3-8)as a cathode material for intermediate temperature solid oxide fuel cells,” Mat. Res. Soc. Symp. Proc. (2004) 801:113-118.
Gut, B. et al., “Anode supported PEN for SOFC. Pressed substrates for spray pyrolysed and co-sintered electrolyte; redox stability and alternative anode,” Jahresbericht (2001) 1-6.
Klemensø, T. et al., “The mechanism behind redox instability of anodes in high-temperature SOFCs,” Electrochemical Society Journal (2005) 152(11):A2186-A2192.
Matus, Y. et al., “Metal-supported solid oxide fuel cell membranes for rapid thermal cycling,” Solid State Ionics (2005) 176:443-449.
Nadler, J.H. et al., “Oxide reduction and sintering of Fe-Cr alloy honeycombs,” J. Mat. Research (2003) 18(8):1787-1794.
Zhang, Y. et al., “Redox cycling of Ni-YSZ anode investigated by TPR technique,” Solid State Ionics (2005) 176:2193-2199.
International Search Report and Written Opinion from International Searching Authority for PCT/DK2005/000379 dated Dec. 16, 2005 (14 pages).
European Patent Office Search Report for European Application No. 062024339 dated Feb. 2, 2007 (2 pages).
International Search Report and Written Opinion from International Searching Authority for PCT/EP2005/013968 dated Mar. 28, 2006 (10 pages).
International Preliminary Report on Patentability from International Searching Authority for PCT/EP2005/013968 dated Mar. 30, 2007 (10 pages).
International Search Report and Written Opinion from International Searching Authority for PCT/EP2006/000229 dated Mar. 15, 2006 (9 pages).
International Search Report and Written Opinion from International Searching Authority for PCT/EP2006/000920 dated Sep. 22, 2006 (10 pages).
International Search Report and Written Opinion from International Searching Authority for PCT/EP2006/000813 dated Mar. 29, 2006 (10 pages).
International Preliminary Report on Patentability from International Searching Authority for PCT/EP2006/000813 dated May 18, 2007 (10 pages).
United States Office Action for U.S. Appl. No. 11/814,356 dated May 1, 2008 (7 pages).
International Search Report from International Searching Authority for PCT/EP2006/008537 dated Aug. 8, 2007 (3 pages).
Notice of Allowability with Office Action for U.S. Appl. No. 11/814,356 dated Jul. 6, 2009 (7 pages).
United States Office Action for U.S. Appl. No. 11/814,356 dated Jan. 2

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Solid oxide fuel cell does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Solid oxide fuel cell, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Solid oxide fuel cell will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4233281

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.