ABSTRACT:
The present invention resides in a die casting process using a solid lubricant composition. The lubricant composition preferably comprises (a) about 30% to about 70% by weight of a high melting point synthetic wax having a melting point in the range of about 270.degree. F. to about 310.degree. F. (132.degree.-154.degree. C.); (b) about 10 to about 50% by weight of a wax having a lower melting point in the range of about 150.degree. F. to about 250.degree. F. (65.degree.-121.degree. C.).

REFERENCES:
patent: 2923041 (1960-02-01), Ryznar
patent: 3645319 (1972-02-01), Pondelicek et al.
patent: 3779305 (1973-12-01), Pondelicek et al.
patent: 3830280 (1974-08-01), Larsen
patent: 4923624 (1990-05-01), Albanesi

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Solid lubricant for die casting process does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Solid lubricant for die casting process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Solid lubricant for die casting process will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1503120

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.