ABSTRACT:
A non-yellowing, elastomeric polyurethane is made from a non-aromatic diisocyanate, a diol chain extender, a polyglycol and an aminodiol chain extender. The polyurethane is stable to sterilizing radiation, is made without any processing aids or toxic catalysts, and softens without swelling up to 95% when contacted with an aqueous liquid.
REFERENCES:
patent: 4822827 (1989-04-01), Bonk et al.
Lambert James M.
Onwunaka Theophilus O.
Becton Dickinson and Company
Brown Richard E.
Welsh Maurice J.
LandOfFree
Softening non-swelling polyurethane does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Softening non-swelling polyurethane, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Softening non-swelling polyurethane will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2097568