ABSTRACT:
Soft copper alloy conductors having a 0.2% proof stress of 12 kg/mm.sup.2 or less which contains 5-200 p.p.m. of calcium, the balance substantially consisting of copper, and hot-dip coated copper alloy conductors made by coating the surface of copper alloy conductors of said composition with tin or lead or their alloy by hot-dipping, and a method of manufacturing said copper alloy conductors.
REFERENCES:
patent: 990040 (1911-04-01), Franke
patent: 1169392 (1916-01-01), Frary
patent: 2202150 (1940-05-01), Hensel et al.
patent: 4059437 (1977-11-01), Nesslage et al.
patent: 4118256 (1978-10-01), Schmitt-Thomas et al.
Rutledge L. Dewayne
Skiff Peter K.
Sumitomo Electric Industries Ltd.
LandOfFree
Soft copper alloy conductors does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Soft copper alloy conductors, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Soft copper alloy conductors will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1689280