ABSTRACT:
Cams which meet all strength requirements and can be shrunk on a shaft can be made in a simple manner by sintering from a nickel- and copper-free mixture which comprises iron powder and contains 0.3 to 1.0 weight percent carbon and molybdenum and/or tungsten in such amounts that the sum of the molybdenums content and the tungsten content multiplied with the ratio of the atomic weight of molybdenum to the atomic weight of tungsten lies between 0.5 and 3 weight percent.

REFERENCES:
patent: 4236923 (1980-12-01), Takahashi
patent: 4595556 (1986-06-01), Umeha et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Sintered shrink-on cam and process of manufacturing such cam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Sintered shrink-on cam and process of manufacturing such cam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Sintered shrink-on cam and process of manufacturing such cam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1799877

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.