ABSTRACT:
A specific composition range and process sequence are described for the production of single crystal superalloy articles which have an exceptional combination of high temperature mechanical properties and resistance to oxidation and hot corrosion. The nominal composition in weight percent is 7.5% Cr, 5.0% Al, 1.0% Ti, 2.0% Mo, 4.0% W, 12.0% Ta, 5% Co, balance nickel. Material of this composition is cast and solidified in single crystal form and heat treated to produce an optimum microstructure.
REFERENCES:
patent: 4222794 (1980-09-01), Schweizer et al.
Duhl David N.
Nguyen-Dinh Xuan
Dean R.
Sohl Charles E.
United Technologies Corporation
LandOfFree
Single crystal nickel superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Single crystal nickel superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Single crystal nickel superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2406852