ABSTRACT:
A single crystal nickel-base superalloy is disclosed having an improved incipient melting temperature and oxidation resistance. The single crystal nickel-base alloy of this invention is characterized by specific addition of chromium, tungsten, aluminum and tantalum to produce an alloy having moderate high temperature strength and improved oxidation resistance and incipient melting temperature. The nominal composition of our new single crystal alloy (in weight percent) is 10-15% Cr, 0-4% Co, 6-8.5% W, 6-7% Al, 0-1% Ti, 2-6% Ta, and the balance nickel.

REFERENCES:
patent: 3026198 (1962-03-01), Thielenann
patent: 3494709 (1970-02-01), Piearcey
patent: 3615376 (1971-10-01), Ross
patent: 3677835 (1972-07-01), Tien et al.
patent: 3756809 (1973-09-01), Asgar
patent: 4045255 (1977-08-01), Jackson
patent: 4058415 (1977-11-01), Walter
patent: 4092183 (1978-05-01), Grundy
patent: 4116723 (1978-09-01), Gell et al.
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4207098 (1980-06-01), Shaw
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4402772 (1985-09-01), Duhl et al.
patent: 4582548 (1986-04-01), Harris et al.
patent: 4583608 (1986-04-01), Field et al.
patent: 4643782 (1987-02-01), Harris et al.
patent: 4677035 (1987-06-01), Fiedler et al.
patent: 4719080 (1988-01-01), Duhl et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Single crystal nickel-base superalloy for turbine components does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Single crystal nickel-base superalloy for turbine components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Single crystal nickel-base superalloy for turbine components will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1508380

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.