ABSTRACT:
A nickel-base superalloy, particularly adapted for use in gas turbine engine single crystal blades and vanes is provided with a specific composition and heat treated in a particular manner to exhibit an improved balance of critical high temperature mechanical properties and resistance to oxidation and hot corrosion significantly superior to presently available alloys. In its broad form, the alloy composition comprises, by weight, 7-12% Cr, 1-5% Mo, 3-5% Ti, 3-5% Al, 5-15% Co, 3-12% W, up to 10% Re, 2-6% Ta, up to 2% Cb, up to 3% V, up to 2% Hf, the balance being essentially nickel and incidental impurities. Nickel-base superalloy single crystal articles formed of the alloy are described, as is the method, including heat treatment, employed to make the article.
REFERENCES:
patent: 3260505 (1966-07-01), Ver Snyder
patent: 3494709 (1977-02-01), Piearcey
patent: 3619182 (1971-11-01), Bieber et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4152488 (1979-05-01), Schilke et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4261742 (1981-04-01), Coupland et al.
patent: 4371404 (1983-02-01), Duhl et al.
patent: 4402772 (1983-09-01), Duhl et al.
patent: 4459160 (1984-07-01), Meetham
patent: 4582548 (1986-04-01), Harris et al.
patent: 4639280 (1987-01-01), Fredholm et al.
patent: 4643782 (1987-02-01), Harris et al.
patent: 4719080 (1988-01-01), Duhl et al.
DE2821524, Dec. 1978.
DE3023576, Jul. 1987.
DE3234083, Apr. 1983.
GE-Final Report-"Directional Solidification Alloy Development"-No. NADC-78136-60, made under Contract No. N62269-78-C-0315 to Dept. of Navy (1 Sep. 1978-1 Jan. 1980).
Buchakjian, Jr. Leo
Wukusick Carl S.
Dean R.
General Electric Company
Phipps Margery S.
Squillaro Jerome C.
Strunk Stephen S.
LandOfFree
Single crystal nickel-base superalloy article and method for mak does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Single crystal nickel-base superalloy article and method for mak, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Single crystal nickel-base superalloy article and method for mak will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1298785