ABSTRACT:
This invention discloses a novel shielding gas mixture for use in gas shielded arc welding processes. The shielding gas of this invention may be used in a wide variety of processes when welding various superalloy compositions. In the broad range, the composition contains, in percent by volume, 5 to 12 helium, 0.1 to 0.9 carbon dioxide and the balance argon. The typical composition contains about 10 helium, about 0.25 to 0.55 carbon dioxide and the balance argon plus impurities.

REFERENCES:
patent: 2591926 (1952-04-01), Gibson et al.
patent: 2753427 (1956-07-01), Yenni et al.
patent: 3042484 (1962-07-01), Maring
patent: 3139506 (1964-06-01), Wolff et al.
patent: 3469304 (1969-09-01), Medsker
patent: 3470346 (1969-09-01), Duboz
patent: 3496323 (1970-02-01), Lesnewich et al.
patent: 4463243 (1984-07-01), Church
patent: 4749841 (1988-07-01), Galantino et al.
patent: 4857692 (1989-08-01), Larson et al.
patent: 4871898 (1989-10-01), Cherne et al.
patent: 4973822 (1990-11-01), Evans et al.
patent: 4999474 (1991-03-01), Schultz et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Shielding gas mixture for welding superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Shielding gas mixture for welding superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Shielding gas mixture for welding superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-116974

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.