Selective flocculation for iron values

Classifying – separating – and assorting solids – Precedent preparation of items or materials to facilitate... – Selective differentiation

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

210734, B03D 306

Patent

active

042820871

ABSTRACT:
An iron ore is finely ground and slurried prior to being subjected to treatment with a selective flocculant for iron values. Subsequent to treatment, the iron values are allowed to settle into the underflow concentrate and be recovered. The selective flocculant employed is a hydroxymethylated polyacrylamide having a high molecular weight and a degree of hydroxymethylation in excess of about 50%.

REFERENCES:
patent: 3418237 (1968-12-01), Booth
patent: 3479282 (1969-11-01), Chamot
patent: 3975496 (1976-08-01), Smalley
patent: 4081357 (1978-03-01), Werneke
patent: 4090955 (1978-05-01), Dexter
patent: 4137164 (1979-01-01), Coscia

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Selective flocculation for iron values does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Selective flocculation for iron values, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Selective flocculation for iron values will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-238806

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.