ABSTRACT:
An improved scale conditioning composition and method is disclosed that results in improved dissolution and disruption of tube scale, hardened sludge and other deposits composed primarily of highly densified magnetite such as those found in heat exchange vessels, particularly steam generators. After treatment with the advanced scale conditioning composition, these magnetite rich deposits are more easily removed using known and commercially available high pressure hydro-mechanical cleaning techniques. The present invention further provides effective cleaning in a short period of time and at relatively low temperatures, while reducing the amount of waste produced and reducing the resulting corrosion of carbon and low alloy steel components within the steam generator during the cleaning process.
REFERENCES:
patent: 3996062 (1976-12-01), Frost et al.
patent: 4045253 (1977-08-01), Banks et al.
patent: 4578162 (1986-03-01), McIntyre et al.
patent: 4586961 (1986-05-01), Bradley et al.
patent: 4632705 (1986-12-01), Baum
patent: 4899697 (1990-02-01), Franklin et al.
patent: 4921662 (1990-05-01), Franklin et al.
patent: 4972805 (1990-11-01), Weems
patent: 5006304 (1991-04-01), Franklin et al.
patent: 5019329 (1991-05-01), Franklin et al.
patent: 5092280 (1992-03-01), Franklin et al.
patent: 5092355 (1992-03-01), Cadwell et al.
patent: 5601657 (1997-02-01), Baum
patent: 4720306 (1998-01-01), Emmert et al.
patent: 5764717 (1998-06-01), Rootham
patent: 5779814 (1998-07-01), Fellers, Sr. et al.
patent: 5814204 (1998-09-01), D'Muhala
patent: 5841826 (1998-11-01), Rootham et al.
patent: 6017399 (2000-01-01), Fellers, Sr. et al.
patent: 6740168 (2004-05-01), Rootham et al.
W. Frenier and F. Growcock, ““Mechanism of Iron Oxide Dissolution—A Review of Recent Literature”,” Corrosion, vol. 40 (No. 12), p. 663-668, (Dec. 23, 1984).
Rootham Michael W.
Varrin Robert D
Dominion Engineering Inc.
Pillsbury Winthrop Shaw & Pittman LLP
Webb Gregory
LandOfFree
Scale conditioning agents and treatment method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Scale conditioning agents and treatment method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Scale conditioning agents and treatment method will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2812026