ABSTRACT:
A room temperature setting carbonaceous cement comprising a solid carbonaceous material, a catalyst, a liquid carbonizable component, and copper particles, which when treated with the catalyst will provide a carbon yield of at least 40% for the liquid component at an elevated baking temperature and possess increased flexural strength at elevated temperatures and reduced electrical resistance.

REFERENCES:
patent: 3441529 (1969-04-01), Tyler
patent: 3979218 (1976-09-01), Hesse et al.
patent: 4001104 (1977-01-01), Vadla et al.
patent: 4915874 (1990-04-01), Nadkorni et al.
patent: 5002981 (1991-03-01), Chiu
patent: 5280063 (1994-01-01), Lewis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Room temperature setting carbonaceous cement with increased elec does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Room temperature setting carbonaceous cement with increased elec, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Room temperature setting carbonaceous cement with increased elec will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1056667

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.