Room temperature cured elastomer

Chemistry of carbon compounds – Miscellaneous organic carbon compounds – C-metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

149 199, 526 476, C08F 800, C08F 802

Patent

active

041246578

ABSTRACT:
Hydroxy terminated polybutadiene is reacted with naphthyl-potassium and 1omo-2,4-pentadiene in successive steps to form a bis(1,3-pentadienyl ether) derivative. Then the bismaleimide of dimer diamine is added to the polybutadiene derivative whereby a room temperature cure to an elastomer is achieved.

REFERENCES:
patent: 3758426 (1973-09-01), Boivin et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Room temperature cured elastomer does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Room temperature cured elastomer, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Room temperature cured elastomer will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2233754

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.