ABSTRACT:
A room temperature vulcanizable silicone rubber composition is prepared by mixing hydroxyl or alkoxyl endblocked polydiorganosiloxane, crosslinking agent containing at least two water-hydrolyzable radicals, namely alkoxy, ketoximo, alkenyloxy, aminoxy, amino, and amido, and a spindle-shaped calcium carbonate. Curing the composition results in a silicone rubber with improved thermal stability.
REFERENCES:
patent: 3957714 (1976-05-01), Clark et al.
patent: 4247445 (1981-01-01), Smith et al.
patent: 4356116 (1982-10-01), Beers
Fukayama Miyoji
Ishida Tadao
Borrousch Roger H.
Briggs Sr. Wilbert J.
Toray Silicone Company Ltd.
LandOfFree
Room temperature curable polyorganosiloxane composition containi does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Room temperature curable polyorganosiloxane composition containi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Room temperature curable polyorganosiloxane composition containi will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-122163