ABSTRACT:
A room temperature-curable organopolysiloxane composition which does not suffer from surface fissuring even when subjected to external stress (e.g., tensile stress, flexural stress) during the course of its cure was prepared and has a composition of a hydroxyl-terminated polydiorganosiloxane, a hydrophobic silica with a silanol titer not exceeding 2.0 mL, a dry-method silica with a silanol titer of at least 5.0 mL, and an oxime group-containing silane or siloxane.
REFERENCES:
patent: 3037933 (1962-06-01), Wright
patent: 4101499 (1978-07-01), Herzig
patent: 4104239 (1978-08-01), Bargain et al.
patent: 4384068 (1983-05-01), Bouverot et al.
patent: 4912153 (1990-03-01), Jeremias et al.
patent: 4956436 (1990-09-01), Letoff et al.
patent: 5023288 (1991-06-01), Hirai et al.
patent: 5145932 (1992-09-01), Sasaki et al.
European Search Report for EP 92 101478 Datum/Date Sep. 8, 1992.
European Abstract 449651.
European Abstract 25092.
Fukayama Miyoji
Ishida Tadao
Suganuma Noriyuki
Bleutge John C.
Borrousch Roger H.
Dean Karen A.
Dow Corning Toray Silicone Ltd.
LandOfFree
Room temperature-curable organopolysiloxane composition does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Room temperature-curable organopolysiloxane composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Room temperature-curable organopolysiloxane composition will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-578118