ABSTRACT:
The room temperature-curable organopolysiloxane composition of the invention is characteristic in the remarkably increased adhesive bonding strength of the rubber of the composition to the surface of a substrate of metals, plastics and others on which the composition has been cured. The composition is also advantageous in the improved thixotropy despite the admixture of an adhesion improver mentioned below. Thus, the composition comprises, in addition to conventional components in a deacidification type room temperature curable organopolysiloxane composition, a specific organic silicon compound represented by the general formula

REFERENCES:
patent: 3109826 (1963-11-01), Smith
patent: 4434283 (1984-02-01), Sattlegger et al.
patent: 4523001 (1985-06-01), Swiger

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Room temperature-curable organopolysiloxane composition does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Room temperature-curable organopolysiloxane composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Room temperature-curable organopolysiloxane composition will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1618162

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.