ABSTRACT:
A sulfide containing copper and one or more of iron, nickel and cobalt, is dead-roasted at a temperature of 750.degree. C or above, then subjected to a pressure leach under reducing conditions to produce elemental copper and an aqueous solution of the other metals.

REFERENCES:
patent: 790238 (1905-05-01), Wilcox
patent: 2716588 (1955-08-01), Hall
patent: 2796342 (1957-06-01), Schaufelberger et al.
patent: 2817583 (1957-12-01), Schlecht et al.
patent: 3573896 (1971-04-01), Hori et al.
patent: 3684489 (1972-08-01), Emicke et al.
patent: 3744994 (1973-07-01), Emicke et al.
patent: 3839013 (1974-10-01), Turkdogan et al.
patent: 4067952 (1978-01-01), Pittie et al.
Shirts et al., Bureau of Mines Report of Investigations 7996, (1975).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Roast-reductive leach process for copper recovery does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Roast-reductive leach process for copper recovery, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Roast-reductive leach process for copper recovery will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2271356

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.