ABSTRACT:
A method is provided for enhancing the neutralization capability of high-magnesium serpentine silicate ore in the neutralization of nickel-containing pregnant leach solution, said solution having a pH of less than about 1 which comprises, providing said high magnesium serpentine ore in particulate form containing by weight over about 5% magnesium, roasting said ore under oxidizing conditions at a temperature below that temperature at which forsterite in said ore recrystallizes, and then adding an amount of said serpentine roasted ore to said pregnant liquor sufficient to raise the pH of the leach solution to a level above 2.

REFERENCES:
patent: 2384008 (1945-09-01), Brandenburg
patent: 3466144 (1969-09-01), Kay
patent: 3991159 (1976-11-01), Queaneau et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Roast-neutralization-leach technique for the treatment of lateri does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Roast-neutralization-leach technique for the treatment of lateri, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Roast-neutralization-leach technique for the treatment of lateri will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2304507

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.