ABSTRACT:
A copper-containing sulfidic material is dead-roasted at a temperature of at least 750.degree. C. and the resulting calcine is leached in a sulfuric acid solution to dissolve most of the copper in preference to any iron, nickel and cobalt in the material.

REFERENCES:
patent: 1634497 (1927-07-01), Greenawalt
patent: 2783141 (1957-02-01), Foley
patent: 2817583 (1957-12-01), Schlecht et al.
patent: 3524802 (1970-08-01), Clevenger
patent: 3751240 (1973-08-01), Green
patent: 3839013 (1974-10-01), Tukdogan et al.
patent: 3883344 (1975-05-01), Griffith
patent: 3959437 (1976-05-01), Rastas et al.
Shirts et al., "Double Roast-Leach Electrowinning Process for Chalcopyrite Concentrates", U.S. Bureau of Mines R.I7996 (1975).
Quenean, Editor, Extractive Metallurgy of Copper, Nickel, Cobalt Interscience Publishers, N.Y., 1961, p. 26, [TN780M4].

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Roast-leach copper recovery does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Roast-leach copper recovery, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Roast-leach copper recovery will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-896994

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.