Rhodium-containing superalloy coatings and methods of making sam

Metal working – Means to assemble or disassemble – Puller or pusher means – contained force multiplying operator

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

427383, 427405, 427253, 204 38S, C23C 902, C23F 1700

Patent

active

039619109

ABSTRACT:
Superalloy structures, such as high temperature components for jet engines and the like, are provided with aluminum-containing diffusion coatings enabling guantum extensions of service life through unique distributions therein of rhodium. The rhodium is prediffused into the alloy structure, and the resultant distribution minimizes aluminum migration into the structure and thus maximizes protective coating performance.

REFERENCES:
patent: 3494748 (1970-02-01), Todd
patent: 3677789 (1972-07-01), Bungardt et al.
patent: 3692554 (1972-09-01), Bungardt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Rhodium-containing superalloy coatings and methods of making sam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Rhodium-containing superalloy coatings and methods of making sam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Rhodium-containing superalloy coatings and methods of making sam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1095297

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.