Metal treatment – Compositions
Patent
1992-03-16
1993-09-07
Rosenberg, Peter D.
Metal treatment
Compositions
252 28, B23K 3534
Patent
active
052425061
ABSTRACT:
A rheologically controlled glass lubricant for hot metal working comprises a glass powder, a binder, a rheological agent, and a wetting and viscosity modifier. These materials may be dispersed in a carrier. The lubricant is made by mixing the constituent elements, milling the mixture, and stabilizing the milled mixture. The lubricant can be used in a forging operation by coating a metal part with the lubricant, heating the coated part, placing the coated heated part in a forge, and rapidly applying sufficient pressure to deform the coated metal part into a desired shape.
REFERENCES:
patent: 3459602 (1969-08-01), Mueller
patent: 3635068 (1972-01-01), Watmough et al.
patent: 4096076 (1978-06-01), Spiegelberg
patent: 4228690 (1980-10-01), Corti et al.
patent: 4281528 (1981-08-01), Spiegelberg et al.
patent: 4571983 (1986-02-01), Sanborn et al.
Barber Raymond J.
Dorrell David R.
Rosenberg Peter D.
Sohl Charles E.
United Technologies Corporation
LandOfFree
Rheologically controlled glass lubricant for hot metal working does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Rheologically controlled glass lubricant for hot metal working, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Rheologically controlled glass lubricant for hot metal working will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-484585