Stock material or miscellaneous articles – All metal or with adjacent metals – Composite; i.e. – plural – adjacent – spatially distinct metal...
Patent
1995-06-07
1998-07-21
Phipps, Margery
Stock material or miscellaneous articles
All metal or with adjacent metals
Composite; i.e., plural, adjacent, spatially distinct metal...
148512, 148527, 428637, B32B 1500
Patent
active
057833184
ABSTRACT:
A repaired nickel-based superalloy substrate that has applied thereon a nickel-based polycrystalline repair alloy comprising 0.03-2.5 weight % hafnium, 0.003-0.32% boron, 0.02-0.16% yttrium and 0.007-0.35% zirconium. The present invention further provides a repaired single crystal alloy substrate that has applied thereon a repair alloy wherein the repair alloy's composition is similar to or the same as the single crystal alloy composition except that the repair alloy additionally comprises at least one grain boundary strengthener element and at least one element that enhances oxidation resistance.
REFERENCES:
patent: 3479157 (1969-11-01), Richards et al.
patent: 3516826 (1970-06-01), Ward et al.
patent: 3617685 (1971-11-01), Brill-Edwards
patent: 3711337 (1973-01-01), Sullivan et al.
patent: 3807993 (1974-04-01), Dalai et al.
patent: 3832167 (1974-08-01), Shaw et al.
patent: 3928026 (1975-12-01), Hecht et al.
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4054723 (1977-10-01), Higginbotham et al.
patent: 4073639 (1978-02-01), Duvall et al.
patent: 4078951 (1978-03-01), Denzine et al.
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4340425 (1982-07-01), Barrett et al.
patent: 4705203 (1987-11-01), McComas et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4743514 (1988-05-01), Strangman et al.
patent: 4820356 (1989-04-01), Blackburn et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
patent: 4849030 (1989-07-01), Darolia et al.
patent: 4878953 (1989-11-01), Salzman et al.
patent: 4961818 (1990-10-01), Benn
patent: 4983233 (1991-01-01), Henry
patent: 5037495 (1991-08-01), Henry
patent: 5043138 (1991-08-01), Darolia et al.
patent: 5068084 (1991-11-01), Cetel et al.
patent: 5069873 (1991-12-01), Harris et al.
patent: 5071059 (1991-12-01), Heitman et al.
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5104614 (1992-04-01), Ducrocq et al.
patent: 5143563 (1992-09-01), Krueger et al.
patent: 5151249 (1992-09-01), Austin et al.
patent: 5156321 (1992-10-01), Liburdi et al.
patent: 5171380 (1992-12-01), Henry
patent: 5173255 (1992-12-01), Ross et al.
patent: 5240491 (1993-08-01), Budinger
patent: 5270123 (1993-12-01), Walston
patent: 5316866 (1994-05-01), Goldman et al.
patent: 5395584 (1995-03-01), Berger et al.
Metals Handbook, 9th Ed. vol. 15, pp. 815-819; STIC TA 472.A3, 1988.
Biondo Charles M.
Gostic William J.
Parmley Christopher D.
Tanzola John C.
Phipps Margery
United Technologies Corporation
LandOfFree
Repaired nickel based superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Repaired nickel based superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Repaired nickel based superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1645140