Repair of glass laminates

Coating processes – Restoring or repairing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

156 94, 264 36, 427163, 427294, 428 63, B32B 3500

Patent

active

041653971

ABSTRACT:
Repair of bulls-eye mark damage to laminated glass is effected by subjecting the area of the crack to reduced air pressure of at most 0.5 mm Hg for 10 minutes, application of a low viscosity, liquid, curable composition, increase in the air pressure, and cure of the resin composition to a transparent polymer.

REFERENCES:
patent: 3562366 (1971-02-01), Sohl
patent: 3765975 (1973-10-01), Holingsworth
patent: 3841932 (1974-10-01), Forler et al.
patent: 3914145 (1975-10-01), Forler et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Repair of glass laminates does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Repair of glass laminates, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Repair of glass laminates will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1323944

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.