ABSTRACT:
Novel materials and methods for repairing/reclassifying superalloy components are described herein. These materials are non-traditional blends of materials having a much higher base material content than traditional repair/reclassification materials. In embodiments used to repair/reclassify nickel-based components, these materials may comprise about 5-18.9 weight percent of a low melting point alloy and about 81.1-95 weight percent of a base material. In embodiments used to repair/reclassify cobalt-based components, these materials may comprise about 15-30 weight percent of a low melting point alloy and about 70-85 weight percent of a base material. These materials can be used to repair surface defects and/or build up worn or eroded areas of a component to meet precise dimensional and metallurgical requirements. These materials create robust repaired components having a dense, isothermally solidified structure having minimal borides and a high re-melt temperature.

REFERENCES:
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4028787 (1977-06-01), Cretella et al.
patent: 4073639 (1978-02-01), Duvall et al.
patent: 4493451 (1985-01-01), Clark et al.
patent: 4705203 (1987-11-01), McComas et al.
patent: 4726101 (1988-02-01), Draghi et al.
patent: 5142778 (1992-09-01), Smolinski et al.
patent: 5437737 (1995-08-01), Draghi et al.
patent: 5522134 (1996-06-01), Rowe et al.
patent: 5549767 (1996-08-01), Pietruska et al.
patent: 5735448 (1998-04-01), Draghi et al.
patent: 5741378 (1998-04-01), Pietruska et al.
patent: 5806751 (1998-09-01), Schaefer et al.
patent: 5922150 (1999-07-01), Pietruska et al.
patent: 6004683 (1999-12-01), Rafferty et al.
patent: 6049978 (2000-04-01), Arnold
patent: 6093368 (2000-07-01), Rafferty et al.
patent: 6503349 (2003-01-01), Pietruska et al.
patent: 6571472 (2003-06-01), Berry et al.
patent: 6725540 (2004-04-01), Bose et al.
patent: 6742698 (2004-06-01), Shah et al.
patent: 2005/0098243 (2005-05-01), Budinger et al.
patent: 2005/0274009 (2005-12-01), Powers
patent: 2006/0049236 (2006-03-01), Minor et al.
patent: 0 836 904 (1998-04-01), None
patent: 836904 (1998-04-01), None
patent: 1 258 312 (2002-11-01), None
patent: 1 491 283 (2004-12-01), None
European Search Report dated Jun. 8, 2006.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Repair and reclassification of superalloy components does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Repair and reclassification of superalloy components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Repair and reclassification of superalloy components will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2790608

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.