ABSTRACT:
A process for producing a low iron nickel base superalloy having a very low selenium content. The process includes the steps of: preparing a superalloy melt containing, by weight, at least 60% nickel, no more than 1% iron, and more than 0.0004% selenium; maintaining the melt in contact with a calcium and/or magnesium bearing substance for a period of time sufficient to allow for reaction between selenium and calcium and/or magnesium, and a lowering of said melt's selenium content to a level below 0.0003%, said selenium removal being carried out in a substantially oxygen free atmosphere; casting the melt; and heat treating the cast metal.

REFERENCES:
patent: 3853540 (1974-12-01), Schlatter et al.
patent: 3891425 (1975-06-01), McCarty

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Refining nickel base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Refining nickel base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Refining nickel base superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-669393

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.