ABSTRACT:
A magnetic memory element has reduced Néel coupling between a pinned layer and a free layer. The magnetic memory element includes a first pinned ferromagnet and a free ferromagnet which are separated by a barrier layer. The magnetic field direction of the pinned layer is fixed, for example, by an antiferromagnetic exchange layer. An additional ferromagnetic layer, provided in coupling relationship with the first pinned ferromagnet, offsets Néel coupling between the free ferromagnetic layer and the first pinned ferromagnet.
REFERENCES:
patent: 5764567 (1998-06-01), Parkin
patent: 6466419 (2002-10-01), Mao
patent: 6714444 (2004-03-01), Huai et al.
patent: 2002/0030489 (2002-03-01), Lenssen et al.
patent: 2002/0141120 (2002-10-01), Gill
Dickstein , Shapiro, Morin & Oshinsky, LLP
Micro)n Technology, Inc.
Nelms David
Tran Mai-Huong
LandOfFree
Reducing the effects of neel coupling in MRAM structures does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Reducing the effects of neel coupling in MRAM structures, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Reducing the effects of neel coupling in MRAM structures will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3480970