ABSTRACT:
Stress corrosion cracking of metal weldments in the presence of an aqueous alkanol amine solution is reduced by the use of a stress corrosion inhibiting amount of a sulfiding agent selected from elemental sulfur or a sulfide ion yielding compound.
REFERENCES:
patent: 3904537 (1975-09-01), Ripple
patent: 4071470 (1978-01-01), Davidson et al.
patent: 4088735 (1978-05-01), Bratzler et al.
patent: 4096085 (1978-06-01), Holoman et al.
patent: 4100100 (1978-07-01), Clouse et al.
patent: 4102804 (1978-07-01), Clouse et al.
patent: 4295979 (1981-10-01), Sharp et l.
patent: 4350600 (1982-09-01), Sharp et al.
patent: 4431563 (1984-02-01), Krawczyk et al.
Fee Valerie Denise
Maples John S.
Shell Oil Company
LandOfFree
Reducing stress corrosion cracking in treating gases with alkano does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Reducing stress corrosion cracking in treating gases with alkano, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Reducing stress corrosion cracking in treating gases with alkano will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-327931