Chemistry of inorganic compounds – Treating mixture to obtain metal containing compound – Group ivb metal
Patent
1978-07-21
1979-10-30
Carter, Herbert T.
Chemistry of inorganic compounds
Treating mixture to obtain metal containing compound
Group ivb metal
423 82, 423 86, 423140, 423150, 75114, C01G 2304
Patent
active
041728785
ABSTRACT:
Titanium metal values may be recovered from a titanium bearing source such as an ilmenite ore by subjecting the source to a reductive roast, leaching the reduced source with a halogen-containing compound followed by crystallization of the iron halide impurity which is separated from the soluble titanium halide. The soluble titanium halide is then treated with an iron oxide to form titanium dioxide. The yield of titanium dioxide may be greatly improved by effecting the nucleation of the titanium in a manner which comprises adding the iron oxide to the solution without agitation. Upon completion of the nucleation reaction, the solids are then thoroughly dispersed before removing the solid titanium dioxide.
REFERENCES:
patent: 3076692 (1963-02-01), Ruter et al.
patent: 3236596 (1966-02-01), Zingibl et al.
patent: 3407033 (1968-10-01), Ruter et al.
patent: 3825419 (1974-07-01), Chen
patent: 3859077 (1975-01-01), Othmer
patent: 3903239 (1975-09-01), Berkovich
patent: 3929962 (1975-12-01), Shiah
Carter Herbert T.
Hoatson Jr. James R.
Nelson Raymond H.
Page II William H.
UOP Inc.
LandOfFree
Recovery of titanium metal values does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Recovery of titanium metal values, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Recovery of titanium metal values will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-20176