Specialized metallurgical processes – compositions for use therei – Processes – Free metal or alloy reductant contains magnesium
Patent
1978-07-19
1979-12-11
Carter, Herbert T.
Specialized metallurgical processes, compositions for use therei
Processes
Free metal or alloy reductant contains magnesium
75 1T, 75114, 423 82, 423 83, 423 85, 423 86, 423140, 423150, C21B 1500, C01G 2304
Patent
active
041781767
ABSTRACT:
Iron metal values and titanium metal values may be recovered from iron and titanium bearing sources such as ilmenite by subjecting the source to a reductive roast followed by leaching of the reduced source with a halogen-containing compound. Thereafter, the iron halide is crystallized and separated from the soluble titanium halides. One portion of the iron halides is subjected to a reducing step to form metallic iron while a second portion is oxidized, the iron oxides being used to precipitate the titanium as titanium dioxide. The titanium dioxide may then be separated and recovered while the liquid portion is recycled to the leaching zone.
REFERENCES:
patent: 3076692 (1963-02-01), Ruter et al.
patent: 3236596 (1966-02-01), Zirngibl et al.
patent: 3407033 (1968-10-01), Ruter et al.
patent: 3529931 (1970-09-01), Moklebust
patent: 3825419 (1974-07-01), Chem
patent: 3859077 (1975-01-01), Othmer
patent: 3903239 (1975-09-01), Berkovich
patent: 3929962 (1975-12-01), Shiah
Carter Herbert T.
Hoatson Jr. James R.
Nelson Raymond H.
Page II William H.
UOP Inc.
LandOfFree
Recovery of iron and titanium metal values does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Recovery of iron and titanium metal values, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Recovery of iron and titanium metal values will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-309179