Recovery-annealed cold-reduced plain carbon steels and methods o

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 12C, 148 12F, C21D 946

Patent

active

039501906

ABSTRACT:
A plain carbon, cold-reduced flat rolled steel product with yield strengths in an intermediate range and exhibiting good ductility, as well as a method of processing to attain said yield strength and good ductility characteristics without reliance upon the purposeful addition of precipitation strengthening agents.

REFERENCES:
patent: 2814578 (1957-11-01), White
patent: 3591427 (1971-07-01), Hansen, Jr.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Recovery-annealed cold-reduced plain carbon steels and methods o does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Recovery-annealed cold-reduced plain carbon steels and methods o, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Recovery-annealed cold-reduced plain carbon steels and methods o will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-749948

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.