ABSTRACT:
A recording medium for use in various types of cards required to accept printed and written marks has a writing layer exhibiting excellent ink absorption ability and high surface layer strength. The recording medium comprises a base material provided with a coating whose surface has irregular surface cracks and a center-line mean roughness Ra of 0.5 .mu.m-2.5 .mu.m. The formation of the coating layer includes a drying step conducted in two or more stages using a drying temperature in the second stage that is 10.degree. C.-40.degree. C. lower than that in the first stage.
REFERENCES:
patent: 3769063 (1973-10-01), Kizawa
patent: 4075050 (1978-02-01), Takashi et al.
patent: 4481244 (1984-11-01), Haruta et al.
patent: 4496629 (1985-01-01), Haruta et al.
patent: 4544580 (1985-10-01), Haruta et al.
patent: 4572847 (1986-02-01), Haruta et al.
patent: 4663216 (1987-05-01), Toyoda et al.
patent: 4705719 (1987-11-01), Yamanaka et al.
patent: 5085932 (1992-02-01), Fujita et al.
patent: 5215812 (1993-06-01), Kano et al.
patent: 5354601 (1994-10-01), Kamijo et al.
Barr Michael
Beck Shrive
Nisshinbo Industries Inc.
LandOfFree
Recording medium and method of producing the same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Recording medium and method of producing the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Recording medium and method of producing the same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1514556