ABSTRACT:
A contactless method and apparatus for real-time in-situ monitoring of a chemical etching process during etching of at least one wafer in a wet chemical etchant bath are disclosed. The method comprises the steps of providing two conductive electrodes in the wet chemical bath, wherein the two electrodes are proximate to but not in contact with a wafer; monitoring an electrical characteristic between the two electrodes as a function of time in the etchant bath of the at least one wafer, wherein a prescribed change in the electrical characteristic is indicative of a prescribed condition of the etching process; and recording a plurality of values of the electrical characteristic as a function of time during etching. From the plurality of recorded values and corresponding times, instantaneous etch rates, average etch rates, and etching end points may be determined. Such a method and the apparatus therefor are particularly useful in a wet chemical etch station.
REFERENCES:
patent: 2933675 (1960-04-01), Hoelzle
patent: 3163568 (1964-12-01), Mieux
patent: 3553052 (1971-01-01), Jubb, Jr.
patent: 3874959 (1975-04-01), Hoekstra
patent: 3959046 (1976-05-01), Bussmann et al.
patent: 3964956 (1976-06-01), Snyder
patent: 4220508 (1980-09-01), Kotani et al.
patent: 4338157 (1982-07-01), Kanda
patent: 4497699 (1985-02-01), de Wit et al.
patent: 4621037 (1986-11-01), Kanda et al.
patent: 4755442 (1988-07-01), Hasebe et al.
patent: 4793895 (1988-12-01), Kaanta et al.
patent: 4969973 (1990-11-01), Rinck et al.
patent: 4989157 (1991-01-01), Balisky
patent: 4995939 (1991-02-01), Ferenczi et al.
patent: 5071508 (1991-12-01), Scheithauer
patent: 5081421 (1992-01-01), Miller et al.
patent: 5198072 (1993-03-01), Gabriel et al.
patent: 5338390 (1994-08-01), Barbee et al.
Goubau, W. M., "Capacitive Etch Rate Monitor for Dielectric Etching", IBM Technical Disc. Bulletin vol. 31, No. 1, Jun. 1988, 448-449.
Liu et al., "Resistance/Capacitance Methods for Determining Oxide Etch End Point", IBM Technical Disc. Bulletin vol. 16, No. 8, Jan. 1974, 2706-2707.
Hoekstra, J.P., "Establishing End Point During Delineation Process", IBM Technical Disc. Bulletin vol. 16, No. 6, Nov. 1973, 1717-1720.
Bassous et al., "An In-Situ Etch Rate Monitor Controller", IBM Technical Disc. Bulletin vol. 20, No. 3, Aug. 1977, 1232-1234.
Barbee Steven George
Heinz Tony Frederick
Hsiao Yiping
Li Leping
Ratzlaff Eugene Henry
Crockatt Dale M.
Dang Thi
International Business Machines - Corporation
LandOfFree
Real time measurement of etch rate during a chemical etching pro does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Real time measurement of etch rate during a chemical etching pro, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Real time measurement of etch rate during a chemical etching pro will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1173219