ABSTRACT:
A female die part has an upwardly opening die cavity for receiving a male die plunger, a supporting surface around the cavity for a porous batt of fiberous reinforcing material overlying the cavity, and a first shearing edge defining the periphery of the opening for the cavity. Peripheral portions of the batt are clamped to the supporting surface, whereupon the die plunger presses portions of the batt into a mold formed between the male plunger and the sidewalls of the cavity to completely fill the mold. A cutter having a second shearing edge cooperates with the first shearing edge to shear peripheral portions of the batt from the portions overlying the die cavity. The shearing edges in cooperation with the die plunger seal the mold to enable injection of reactive chemicals that impregnate the porous batt within the mold.

REFERENCES:
patent: 3041669 (1962-07-01), Marshall et al.
patent: 3357053 (1967-12-01), Lyon et al.
patent: 3822161 (1974-07-01), Haase
patent: 4216184 (1980-08-01), Thomas
patent: 4269579 (1981-05-01), Thomas
patent: 4466934 (1984-08-01), Cane et al.
patent: 4755129 (1988-07-01), Baker et al.
patent: 4810444 (1989-03-01), Alberino et al.
patent: 4830599 (1989-05-01), Okasaka et al.
patent: 4917902 (1990-04-01), Slocum et al.
patent: 4940557 (1990-07-01), Kimaya
patent: 4986948 (1991-01-01), Komiya et al.
patent: 5085571 (1992-02-01), Congleton

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Reaction injection molding method with internal frame and shear does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Reaction injection molding method with internal frame and shear , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Reaction injection molding method with internal frame and shear will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1350066

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.