Raw coke for electricity storage carbon material and needle...

Chemistry of inorganic compounds – Carbon or compound thereof – Elemental carbon

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C423S448000, C423S460000, C423S461000, C361S502000, C208S014000, C208S023000, C208S113000, C208S131000, C252S502000, C252S510000, C201S006000, C201S025000

Reexamination Certificate

active

07959888

ABSTRACT:
The present invention provides a raw coke having such a structure that the graphitized product resulting from graphitization of the raw coke at a temperature of 2800° C. under an inactive gas atmosphere will have ratios of the crystallite size to the lattice constant of 360 or less in the (002) plane and 1500 or less in the (110) plane, as a raw coke providing active carbon produced by alkali-activating the raw coke, which is reduced in remaining alkali content and can simplify washing operation because washing liquid can easily pass through the activated carbon, or as a raw coke for the production of needle coke.

REFERENCES:
patent: 5900189 (1999-05-01), Kawano et al.
patent: 2004/0131860 (2004-07-01), Tano et al.
patent: 2005/0266990 (2005-12-01), Iwasaki et al.
patent: 2008/0304206 (2008-12-01), Tano et al.
patent: 1 675 141 (2006-06-01), None
patent: 05-105881 (1993-04-01), None
patent: 05-163491 (1993-06-01), None
patent: 05-202362 (1993-08-01), None
patent: 07-003267 (1995-01-01), None
patent: 2002-110157 (2002-04-01), None
patent: 2003-51430 (2003-02-01), None
patent: 2003051430 (2003-02-01), None
patent: 2003-272622 (2003-09-01), None
patent: 2004-185975 (2004-07-01), None
patent: 2004-247433 (2004-09-01), None
patent: 2005-123462 (2005-05-01), None
patent: 1456447 (1989-02-01), None
patent: 2004/011371 (2004-02-01), None
“Prodecure for the measurements of lattice parameters and crystallite sizes of carbon materials by X-ray diffraction”, The 117 Committee of the Japan Society for the Promotion of Sciences, No. 221, pp. 52, (2006).
“Basic Carbonization Engineering” by Yuzo Sanada and Sugiro Otani published by Ohmsha Ltd., pp. 147.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Raw coke for electricity storage carbon material and needle... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Raw coke for electricity storage carbon material and needle..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Raw coke for electricity storage carbon material and needle... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2727864

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.