ABSTRACT:
A radio-photoluminescence dosimeter glass of low energy dependence, high sensitivity, and good resistance to weathering is composed of an activating silver compound such as silver metaphosphate and at least one metal fluoride, preferably of metals of groups I, II, III, and/or IV of the Periodic System. Such a glass may contain at least one further metal oxide, preferably an oxide of metals of groups I, II, and/or III of the periodic System, phosphorus pentoxide, and, if desired, nitrogen pentoxide.

REFERENCES:
patent: 3208860 (1965-09-01), Armistead et al.
patent: 3449136 (1969-06-01), Carpentier et al.
patent: 3554920 (1971-01-01), Becker
patent: 3740241 (1973-06-01), Bromer et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Radio-photoluminescence dosimeter glass of low energy dependence does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Radio-photoluminescence dosimeter glass of low energy dependence, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Radio-photoluminescence dosimeter glass of low energy dependence will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2346170

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.