ABSTRACT:
The present invention is directed to the achievement of increased gas turbine engine efficiencies through further improvements in nickel-base superalloys used to make parts and components for gas turbine engines. The present invention comprises nickel-base superalloys for producing single crystal articles having a significant increase in temperature capability, based on stress rupture strength and low and high cycle fatigue properties, over single crystal articles made from current production nickel-base superalloys. Further, because of their superior resistance to degradation by cyclic oxidation, and their resistance to hot corrosion, the superalloys of this invention possess a balance in mechanical and environmental properties which is unique and has not heretofore been obtained.

REFERENCES:
patent: 3260505 (1966-07-01), Ver Snyder
patent: 3494709 (1970-02-01), Piercey
patent: 3619182 (1971-11-01), Bleber et al.
patent: 3904402 (1975-09-01), Smashey
patent: 4031945 (1977-06-01), Gigliotti
patent: 4116723 (1978-09-01), Gell et al.
patent: 4152488 (1979-05-01), Schilke et al.
patent: 4162918 (1979-07-01), Huseby
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer et al.
patent: 4261742 (1981-04-01), Coupland et al.
patent: 4371404 (1983-02-01), Duhl et al.
patent: 4402772 (1983-09-01), Duhl et al.
patent: 4522664 (1985-06-01), Gigliotti et al.
patent: 4582548 (1986-04-01), Harris et al.
patent: 4589937 (1986-05-01), Jackson et al.
patent: 4639280 (1987-01-01), Fredholm et al.
patent: 4643782 (1987-02-01), Harris et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4849030 (1989-07-01), Durolia et al.
patent: 5043138 (1991-07-01), Darolia et al.
patent: 5077141 (1991-12-01), Nalk et al.
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5399313 (1995-03-01), Ross et al.
patent: 5455120 (1995-10-01), Walston et al.
Metals Handbook vol. 5 8th Ed pp. 237-261, Oct. 1970.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Property-balanced nickel-base superalloys for producing single c does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Property-balanced nickel-base superalloys for producing single c, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Property-balanced nickel-base superalloys for producing single c will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2066019

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.