ABSTRACT:
In a process for the production of a low molecular weight polyanhydride having a softening point within the range of about 111.degree. to 156.degree. C. by the mass polymerization reaction of a maleic monomer and at least one alkyl-substituted styrene at a temperature in the range of about 140.degree. to 200.degree. C., the improvement comprising employing an alkali metal bifluoride, preferably potassium bifluoride, as catalyst for the reaction.

REFERENCES:
patent: 3732332 (1973-05-01), Curtis et al.
patent: 3789038 (1974-01-01), Curtis et al.
patent: 3929738 (1975-12-01), Curtis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Production of low molecular weight polyanhydrides does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Production of low molecular weight polyanhydrides, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Production of low molecular weight polyanhydrides will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-525590

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.