ABSTRACT:
The production of a continuously advancing steel strip with a protective metal coating on only one face thereof by electrolytically depositing a thin primary coating of metal from an ionized metal salt bath onto said face, which is followed by a cleansing and drying thereof. Thereafter a predetermined quantity of coating metal in minute particulate form is deposited uniformly onto the coated face and is heated in a non-oxidizing atmosphere to fuse the particulate metal particles onto the thin primary coating followed by the sudden cooling thereof, while preventing the oxidation of the uncoated face during the fusing and cooling-off stages.
REFERENCES:
patent: 2197622 (1940-04-01), Sendzimir
patent: 2198253 (1940-04-01), Koehring
patent: 3055768 (1962-09-01), Lassiter
patent: 3231971 (1966-02-01), McFarland et al.
patent: 3428472 (1969-02-01), Shimose et al.
patent: 3745034 (1973-07-01), Smith et al.
patent: 4061801 (1977-12-01), Hamada et al.
Beck Shrive P.
Lebowitz Samuel
LandOfFree
Production of heavy metal coatings on only one face of steel str does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Production of heavy metal coatings on only one face of steel str, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Production of heavy metal coatings on only one face of steel str will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1417518